Brand Name : Lonroy
Model Number : LRHY
Certification : Includes Calibration Certification
Place of Origin : China
MOQ : 1
Price : Negotaible
Payment Terms : L/C,D/A,D/P,T/T,Western Union
Supply Ability : 200
Delivery Time : 5-8 work days
Packaging Details : Wooden package
Power Supply : 380V AC, 3kW
Sample Size : Ø50 × 50 mm
Sample Load Pressure : 0.2MPa
Max. Heating Temperature : 1650°C
Warranty : 1 Year
This instrument is used to test the resistance of refractory materials to the high-temperature load softening effect, and it is an important indicator for testing the high-temperature mechanical properties of refractory materials. It complies with the national standards GB/T5073-2005 "Test Method for Creep of Refractory Materials under Pressure" and GB/T5989-2008 "Test Method for Softening Temperature of Refractory Materials under Load", and it can conduct automatic computer testing, data processing, and automatically generate temperature and deformation curve graphs for saving.
2.Technical Parameter
| Parameter Item | Specification |
| Max. Heating Temperature | 1650°C |
| Temperature Control | ±1°C accuracy, microprocessor-programmable |
| Deformation Measurement Error | ≤0.01mm |
| Sample Size | Ø50 × 50 mm |
| Sample Load Pressure | 0.2MPa |
| Power Supply | 380V AC, 3kW |
|
|